Thermal Degradation Mechanism of Long Carbon Chain Heat Resistant Polyamide 10T/66
更新时间:2024-01-31
    • Thermal Degradation Mechanism of Long Carbon Chain Heat Resistant Polyamide 10T/66

    • Engineering Plastics Application   Issue 4, (2019)
    • DOI:10.3969/j.issn.1001-3539.2019.04.019    

      CLC:
    • Published:2019

    移动端阅览

  • Liu Bingxiao, Hu Guosheng, Zhang Jingting, et al. Thermal Degradation Mechanism of Long Carbon Chain Heat Resistant Polyamide 10T/66[J]. Engineering Plastics Application, 2019, (4). DOI: 10.3969/j.issn.1001-3539.2019.04.019.

  •  
  •  

0

Views

4

下载量

5

CSCD

Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Study on Non-isothermal Crystallization Kinetics of Heat Resistant PA10T/66 and PA10T/66/GF Composites
Design of fitting process between automotive polyamide material parts and steel bushs
Preparation of flexible and branched polyamide 6 and its non-isothermal crystallization kinetics
Design of injection mould for multi-directional deep cavity plastic parts of automobile intercooler air chamber
Advances in preparation of bio-based polyamide thermoplastic elastomers

Related Author

LI Qianxi
ZHU Chenhong
ZHAO Shikun
LOU Shuo
XU Yihui
KANG Peng
GAO Dali
YU Wentao

Related Institution

Guangzhou Automobile Group Co.,Ltd. Automotive Engineering Institute
Guangdong Technician College of Light Industry
Science and Technology Department of China Petroleum and Chemical Corporation (Sinopec)
Plastics Processing Research Institute,Beijing Research Institute of Chemical Industry
Ningbo Mingye Auto Parts Co.,Ltd.
0